ASTM A439 - 83(2009) en

Standard Specification for Austenitic Ductile Iron Castings

  • Deze norm is ingetrokken sinds 01-11-2015

50,60 61,23 Incl BTW

Over deze norm

Status Ingetrokken
Aantal pagina's 6
Gepubliceerd op 01-05-2009
Taal Engels

1.1 This specification covers austenitic ductile iron castings, which are used primarily for their resistance to heat, corrosion, and wear, and for other special purposes.

1.2 Austenitic ductile iron, also known as austenitic nodular iron or austenitic spheroidal iron, is characterized by having its graphite substantially in a spheroidal form and substantially free of flake graphite. It contains some carbides and sufficient alloy content to produce an austenitic structure.

1.3 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.