Norm

ISO 105-X11:1994 en

Textiles - Tests for colour fastness - Part X11: Colour fastness to hot pressing

31,57

Over deze norm

Status Definitief
Aantal pagina's 3
Commissie Textiel en kleding
Gepubliceerd op 01-09-1994
Taal Engels
Tests are given for hot pressing when the textile is dry, when it is wet, and when it is damp. The end-use of the textile usually determines which test should be made. A dry specimen (dry pressing) or a dry specimen covered with a wet cotton adjacent fabric (damp pressing) or a wet specimen covered with a wet cotton adjacent fabric (wet pressing) are pressed with a heating device at a specified temperature and pressure for a specified time.