Norm

NEN-EN 4720:2014 en

Aerospace series - Steel X4CrNiMo16-5-1 (1.4418) - Air melted and electroslag remelted (ESR) - Hardened and tempered - Bar - De ≤ 200 mm - 1150 MPa ≤ Rm ≤ 1300 MPa

34,50

Over deze norm

Status Definitief
Aantal pagina's 8
Commissie Lucht- en ruimtevaart
Gepubliceerd op 01-10-2014
Taal Engels
NEN-EN 4720 specifies the requirements relating to: Steel X4CrNiMo16-5-1 (1.4418) Air melted and electroslag remelted (ESR) Hardened and tempered Bar De ≤ 200 mm 1150 MPa ≤ Rm ≤ 1300 MPa for aerospace applications.

Details

ICS-code 49.025.10
Nederlandse titel Aerospace series - Steel X4CrNiMo16-5-1 (1.4418) - Air melted and electroslag remelted (ESR) - Hardened and tempered - Bar - De ≤ 200 mm - 1150 MPa ≤ Rm ≤ 1300 MPa
Engelse titel Aerospace series - Steel X4CrNiMo16-5-1 (1.4418) - Air melted and electroslag remelted (ESR) - Hardened and tempered - Bar - De ≤ 200 mm - 1150 MPa ≤ Rm ≤ 1300 MPa